Laser powder bed fusion of metal alloys

Complex geometries — Structural weight reduction

LPBF builds parts by selectively melting metal powder with a laser, layer by layer. It enables complex geometries while requiring control of supports, orientation, residual stresses and post-processing. Performance must be assessed for the specific application.

WATCHJUNO.AM

Loading this video consents to connecting to YouTube (Google), which receives your IP and technical data and may use storage technologies. It is optional: continue reading without loading it, or stop it at any time. This choice applies only to this video on the current page.

Cookies and external video · Google Privacy

Application-specific mechanical performance

Mechanical properties depend on the alloy, build orientation, process parameters and heat treatment. We evaluate the relevant requirements rather than assuming equivalence with cast or machined parts.

Design freedom, with manufacturing constraints

Layer-wise laser melting enables shapes that are difficult to machine. Minimum features, supports, powder removal and finishing access still influence the design.

Post processing

Heat treatment, HIP, machining and finishing may be appropriate depending on the alloy, geometry and required properties. The post-processing route is defined for the application.

Constantly evolving materials

Atomised metal alloys suitable for additive manufacturing are undergoing a phase of rapid innovation, both in terms of quantity and performance.

MATERIALS

Available alloys

Alloy selection considers the load case, environment, production process and qualification requirements. Post-processing and acceptance criteria are defined for each application.

AlSi10Mg

Aluminium AlSi10Mg

Lightweight structural alloy. Excellent strength-to-weight ratio, good thermal conductivity. Available as built or heat treated.

316L

Stainless Steel 316L

An austenitic stainless steel selected for applications requiring corrosion resistance and ductility. Suitability depends on the environment, finish and applicable requirements.

Ti6Al4V

Titanium Ti6Al4V

A titanium alloy used for demanding lightweight applications. Suitability, material traceability and qualification requirements must be assessed for the intended use.

DATASHEETS

Three production alloys, fully characterised

Mechanical data for our three core LPBF alloys, printed from certified m4p atomised powders on laser powder bed fusion systems. Values are indicative of as-built and heat-treated conditions; we confirm the figures relevant to your part on request.

Powderm4p 316L
ProcessLPBF · Laser Powder Bed Fusion
StandardASTM A276 / DIN EN 10088

Ultimate tensile strength Rm (MPa)

XY direction · 640 ± 30Z direction · 590 ± 30

Yield strength Rp0.2 (MPa)

XY direction · 540 ± 30Z direction · 470 ± 30

Elongation at break A (%)

XY direction · 40 ± 10Z direction · 50 ± 10

Young's modulus (GPa)

XY direction · 190 ± 10Z direction · 190 ± 10

Hardness

XY direction · ≈ 210 HV10Z direction · ≈ 210 HV10

Relative density (%)

XY direction · ≥ 99.7Z direction · ≥ 99.7

Density (g/cm³)

XY direction · ≥ 7.99Z direction · ≥ 7.99
Powderm4p AlSi10Mg
ProcessLPBF · Laser Powder Bed Fusion
StandardDIN EN 1706

Ultimate tensile strength Rm (MPa)

As built (XY) · 445 ± 20As built (Z) · 405 ± 20Heat treated (XY) · 335 ± 20Heat treated (Z) · 325 ± 20

Yield strength Rp0.2 (MPa)

As built (XY) · 275 ± 20As built (Z) · 230 ± 10Heat treated (XY) · 225 ± 20Heat treated (Z) · 220 ± 10

Elongation at break A (%)

As built (XY) · 6.5 ± 2As built (Z) · 3.5 ± 2Heat treated (XY) · 11 ± 2Heat treated (Z) · 7 ± 2

Young's modulus (GPa)

As built (XY) · 70 ± 5As built (Z) · 65 ± 5Heat treated (XY) · 70 ± 5Heat treated (Z) · 65 ± 5

Fatigue strength, Z (MPa)

As built (XY) · 97 ± 7As built (Z) · 97 ± 7Heat treated (XY) · 97 ± 7Heat treated (Z) · 97 ± 7

Hardness

As built (XY) · ≈ 120 HBWAs built (Z) · ≈ 120 HBWHeat treated (XY) · ≈ 120 HBWHeat treated (Z) · ≈ 120 HBW

Density (g/cm³)

As built (XY) · 2.67As built (Z) · 2.67Heat treated (XY) · 2.67Heat treated (Z) · 2.67
Powderm4p Ti64 Grade 23
ProcessLPBF · Laser Powder Bed Fusion
StandardASTM F3001 / F2924

Ultimate tensile strength Rm (MPa)

As built · 1270 ± 50Heat treated · 1040 ± 30

Yield strength Rp0.2 (MPa)

As built · 1120 ± 30Heat treated · 960 ± 30

Elongation at break A (%)

As built · 8.7 ± 2Heat treated · 14.0 ± 2

Young's modulus (GPa)

As built · 110 ± 10Heat treated · 110 ± 10

Hardness

As built · ≈ 360 HVHeat treated · ≈ 360 HV

Density (g/cm³)

As built · 4.42Heat treated · 4.42